SiC Rollers


Specifications

Major Chemical Analysis Al2O3 40~42%
Mineral Phase SiC. Mu.
Density 2.53~2.58 g/cm³
Porosity 19~22 %
Bending strength 670~820 Kgf/cm²
Thermal Expansion 14.35~4.55 x 10-6/℃380
Heat Transfer Coefficient 4.95~5.15 W/mK
Thermal Shock Resistance very good
Max. working Temperature 1100 ℃
Refractoriness Temperature 1350 ℃
Advised uses in tile manufacturer Suitable for all kinds of tiles, special for Rapid Cooling Zone